Danfoss SpeedUp Eco Wall Heating - Dry construction instrukcja

Typ
instrukcja
Application Sheet
SpeedUp Eco Wall Heating
Dry construction with wood battens
Fibre reinforced plasterboard
1 Dry walling screws
2 Wood battens, 30 mm
3 SpeedUp Eco panel, 30 mm
4 Danfoss composite pipe 16 x 2 mm
5 Fibre reinforced plasterboard, 12.5 mm
Technical Data Drywall construction with wood battens
Wall covering 12.5 mm Fibre reinforced plasterboard or similar
Constructional thickness 42.5 mm Dimensions without unfinished wall
Thermal resistance R 0.75 K / W Thermal resistance value for SpeedUp Eco panel
Pipe spacing 125-250 mm EZ = 125; CZ = 250;
Requirements and specialities
Surface smoothness of +/- 3 mm per 1m. Observe building regulation requirements
concerning thermal insulation. Moisture condensation can occur and should be taken
into consideration when planning wall heating on outer walls and walls between heated
and unheated rooms.
Wall coverings
Fermacell/fibre reinforced plasterboard: Thermal conductivity 0.32 W/m²K; maximum
flow temperature 55°C; form board butt joint as glued joint. Form wall attachment with
an elastic acrylic joint or joint filler on divider.
Construction:
Refering to EN 1264
Construction number 612
VAEUN102 © Danfoss 06/2010
1
2
3
4
5
  • Page 1 1

Danfoss SpeedUp Eco Wall Heating - Dry construction instrukcja

Typ
instrukcja